Week12 : Compposites

home up previous next

The Process:

1- Mold preparation :

  • Cleaning both parts(Male/Female) of the mold with water and aceton to remove dust particles.

mold2.jpg

mold1.jpg

  • Mold releas wax applied on both sides twice to allow for easy release of the finnished articles.

wax2.jpg

2- Fiber selection :

  • Isolated the fresh and felxible palm fibers from the dry ones.

fiber5.jpg

fiber0.jpg

fiber1.jpg

fiber2.jpg

3- Layup of the fiber

  • Chopped strand mat

    glassFiber1.jpg

  • Woven Roving 90 degress

    glassFiber2.jpg

4- Lamination

  • With brush idealy with spray but wasn't available
  • I used polyster resin

    lamin1.jpg

    lamin2.jpg

    lamin3.jpg

6- Compression

used weights to compress both sides of the mold

7- Demolding

Date: 2015-03-30

Author: Salman Oraibi @ Fablab-Bahrain

Created: 2016-11-19 Sat 21:50

Emacs 24.5.1 (Org mode 8.2.10)